At normal temperature and humidity, the casting sand mixing ratio suitable for automated molding lines is: mixing ratio (weight ratio) casting old sand 95%, new sand 3%, bentonite 0.8-1.0%, coal powder 0.4-0.5%, water accounts for 3% of the total weight of all materials (not exceeding 3%);